| LOCTITE 079 |
Anaerobic acrylate |
Low |
— |
Small / serviceable fasteners |
Anaerobic |
Serviceable threadlocking |
Low-strength specification / Letter Grade EV |
| LOCTITE 083 |
Anaerobic acrylate |
Medium |
— |
General metal fasteners |
Anaerobic |
Serviceable threadlocking |
Medium-strength specification / Letter Grade CV |
| LOCTITE 084 |
Anaerobic acrylate |
Medium |
10–25 |
Close-fitting threads |
Anaerobic |
Low-viscosity threadlocking |
Very low viscosity / Letter Grade C |
| LOCTITE 087 |
Anaerobic acrylate |
High |
100–250 |
Coarse threaded fasteners |
Anaerobic |
Permanent fastening |
High-strength specification / Letter Grade AV |
| LOCTITE 2047 |
Anaerobic acrylate |
Medium |
— |
General metal fasteners |
Anaerobic |
Serviceable assemblies |
Medium strength with slower cure profile |
| LOCTITE 220 |
Anaerobic acrylate |
Low |
Low / wicking |
Small / preassembled fasteners |
Anaerobic |
Post-assembly locking |
Low-strength wicking grade |
| LOCTITE 222MS |
Anaerobic acrylate |
Low |
Thixotropic |
Small fasteners |
Anaerobic |
Small screws / adjustment fasteners |
Easy hand-tool disassembly |
| LOCTITE 242 |
Anaerobic acrylate |
Medium |
Medium |
General metal fasteners |
Anaerobic |
General industrial assembly |
General-purpose removable threadlocker |
| LOCTITE 2422 |
Anaerobic acrylate |
Medium |
Thixotropic paste |
Metal fasteners |
Anaerobic |
High-temperature assemblies |
High-temperature serviceable grade |
| LOCTITE 2432 |
Anaerobic acrylate |
Medium |
— |
General metal fasteners |
Anaerobic |
General industrial assembly |
Medium-strength threadlocking |
| LOCTITE 246 |
Anaerobic acrylate |
Medium–high |
Medium |
Metal fasteners |
Anaerobic |
Vibration-prone assemblies |
Enhanced vibration resistance |
| LOCTITE 248 |
Anaerobic acrylate |
Medium |
Semi-solid |
Metal threaded fasteners |
Anaerobic |
Portable maintenance |
Clean semi-solid stick application |
| LOCTITE 262 |
Anaerobic acrylate |
Medium–high |
Thixotropic |
Metal fasteners |
Anaerobic |
Heavy-duty fastening |
Controlled thixotropic application |
| LOCTITE 2620 |
Anaerobic acrylate |
Medium–high |
Thixotropic paste |
Metal fasteners |
Anaerobic |
Elevated-temperature assemblies |
High-temperature paste threadlocker |
| LOCTITE 263 |
Anaerobic acrylate |
High |
Low |
Metal fasteners |
Anaerobic |
Permanent threadlocking |
High strength with oil tolerance |
| LOCTITE 266 |
Anaerobic acrylate |
High |
Thixotropic |
Metal fasteners |
Anaerobic |
Permanent fastening |
Oil-tolerant high-strength grade |
| LOCTITE 268 |
Anaerobic acrylate |
High |
Semi-solid |
Metal threaded fasteners |
Anaerobic |
Permanent field assembly |
High-strength stick format |
| LOCTITE 2701 |
Anaerobic acrylate |
High |
Low |
Close-fitting metal fasteners |
Anaerobic |
Permanent locking |
Low viscosity with high strength |
| LOCTITE 271 |
Anaerobic acrylate |
High |
Low |
Large threaded fasteners |
Anaerobic |
Permanent fastening |
High strength for large fasteners |
| LOCTITE 272 |
Anaerobic acrylate |
High |
Medium |
Metal threaded fasteners |
Anaerobic |
High-temperature fastening |
High-temperature high-strength grade |
| LOCTITE 2760 |
Anaerobic acrylate |
High |
— |
Metal fasteners |
Anaerobic |
Rapid permanent fastening |
Fast cure with reduced migration |
| LOCTITE 277 |
Anaerobic acrylate |
High |
Medium |
Large bolts / studs |
Anaerobic |
Heavy equipment fastening |
Designed for large-diameter fasteners |
| LOCTITE 290 |
Anaerobic acrylate |
Medium–high |
Low / wicking |
Preassembled fasteners |
Anaerobic |
Post-assembly locking |
Wicks into assembled threads |
| LOCTITE 294 |
Anaerobic acrylate |
Medium–high |
Low / wicking |
Close-fitting / assembled fasteners |
Anaerobic |
Post-assembly threadlocking |
Low-viscosity wicking grade |
| LOCTITE 962T |
Anaerobic acrylate |
High |
Thixotropic |
Metal threaded fasteners |
Anaerobic |
High-temperature fastening |
High-strength, heat-resistant grade |
| PERMABOND HH120 |
Anaerobic acrylate |
High |
~7,000 |
Coarse / larger threads |
Anaerobic |
Heavy-duty threadlocking |
High-viscosity non-drip formulation |
| PERMABOND HH131 |
Anaerobic acrylate |
Very high |
High / thixotropic |
Bolts, nuts and screws |
Anaerobic |
Permanent high-temperature locking |
High-temperature grade with gas / drinking-water approvals |
| PERMABOND HL126 |
Anaerobic acrylate |
High |
10–30 |
Preassembled / very close-fitting threads |
Anaerobic |
Wicking threadlocking |
Ultra-low-viscosity penetrating grade |
| PERMABOND HM118 |
Anaerobic acrylate |
High |
~1,800 |
Metal threaded fasteners |
Anaerobic |
Permanent industrial fastening |
High-strength general threadlocking |
| PERMABOND HM128 |
Anaerobic acrylate |
High |
~500 |
Metal threaded fasteners |
Anaerobic |
Permanent threadlocking |
High-strength medium-viscosity grade |
| PERMABOND HM129 |
Anaerobic acrylate |
High |
~500 |
Metal threaded fasteners |
Anaerobic |
Permanent threadlocking |
Current Permabond classification is threadlocker |
| PERMABOND LM113 |
Anaerobic acrylate |
Low |
~1,200 |
Small / serviceable fasteners |
Anaerobic |
Frequently dismantled assemblies |
Low strength for easy disassembly |
| PERMABOND MM115 |
Anaerobic acrylate |
Medium |
~1,300 |
General metal fasteners |
Anaerobic |
Serviceable threadlocking |
Controlled medium strength / off-torque |