ROYAL DOUBLE BUBBLE 04006

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

ROYAL DOUBLE BUBBLE 04006

Main features

  • Low-Viscosity Thin-Bondline Flow
  • Extended 45-Minute Working Window
  • Progressive Room-Temperature Strength Build

Product Description

Hardman Double/Bubble 04006 Regular-Setting Epoxy combines a 3.5 g premeasured dual-pouch format with a low-viscosity, two-part epoxy for thin glue lines. The light-amber mixed adhesive has a viscosity of 3,700 cP at 25 deg C, a 45 minute work time, and a 4 hour handling time. It sets in a 10 mil film at room temperature and develops typical lap shear strength from 500 psi after 3 hours to 2,900 psi after two weeks on acid-etched aluminum. The cured material reaches 78 Shore D hardness and is used for furniture, hobby, and sports-equipment repair on supported aluminum, epoxy, phenolic, and wood surfaces.

Key features

  • Thin glue-line flow: The 3,700 cP mixed viscosity is suited to a 10 mil adhesive film.
  • 45-minute work time: The defined working window supports placement before the 4 hour handling stage.
  • Progressive room-temperature strength: Lap shear rises from 500 psi after 3 hours to 2,900 psi after two weeks on acid-etched aluminum.

Applications

Applications include thin glue-line bonding and repair for furniture, hobby projects, and sports equipment using supported aluminum, epoxy, phenolic, and wood surfaces.

Product Family

ROYAL DOUBLE BUBBLE 04006

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Service temperatureService temperature
52 °C

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Package size3.5gPremeasured dual-pouch packet
ColorLight amber-Part A, Part B, and mixed adhesive
Mixed viscosity3,700cPAt 25 deg C
Work time45minAt room temperature
Tack-free time60minAt room temperature
Handling strength4hAt room temperature
Shelf life24monthsPart A and Part B
Technical properties

After processing / final state

Property Value Unit Method / condition
Hardness78Shore DTested at 25 deg C
Impact strength6.7ft-lbTested at 25 deg C
Maximum service temperature52deg CCured adhesive
Lap shear strength500psiAcid-etched aluminum-to-aluminum; 3 h cure at 25 deg C
Lap shear strength2,000psiAcid-etched aluminum-to-aluminum; 24 h cure at 25 deg C
Lap shear strength2,900psiAcid-etched aluminum-to-aluminum; 2 week cure at 25 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers