PP-52008G-060-TSF Nylon Peel Ply
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

Main features
- 100% Nylon 6,6 Peel Ply
- Fine Surface Impression
- FIN 060 Scoured Heat-Set Fabric
Product Description
PP-52008G-060-TSF Nylon Peel Ply is a 100% nylon 6,6 fabric designed for vacuum-bag composite layups and metal-to-metal bonding structures. The peel ply melts at approximately 480°F (249°C) and leaves a fine surface impression after removal to support subsequent priming and secondary bonding operations. The FIN 060 construction has a scoured and heat-set finish and is available in precision-slit widths of 56 inches or less.
Key features
- Nylon 6,6 construction: Manufactured from 100% nylon 6,6 fiber with an approximate melting point of 480°F (249°C).
- Bond-preparation surface: Leaves a fine surface impression suitable for subsequent priming and secondary bonding.
- Scoured and heat-set finish: FIN 060 is supplied with the manufacturer-designated NAT scoured and heat-set finish.
- Precision-slit availability: Available in precision-slit widths of 56 inches or less.
Applications / Suitable for
- Vacuum-bag composite layups
- Metal-to-metal bonding structures
- Surface preparation before priming and secondary bonding
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
Published product properties. The source states that the information is not to be construed as a specification.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Material | 100% nylon 6,6 fiber | — | Code 52008 |
| Finish | FIN 060 – NAT, scoured and heat-set | — | Manufacturer finish designation |
| Fiber melting point | Approximately 480 (249) | °F (°C) | Nylon 6,6 fiber |
| Roll width | 58 (147.3) minimum | in (cm) | ASTM D3774 |
| Roll length | 300 (274.3) maximum | yd (m) | Published roll format |
| Weight | 1.7 (57.6) minimum | oz/yd² (g/m²) | ASTM D3776 |
| Finished count – warp | 101 (39.8) minimum | ends/in (ends/cm) | ASTM D3775 |
| Finished count – fill | 82 (32.3) minimum | picks/in (picks/cm) | ASTM D3775 |
| Tensile strength – warp | 115 (511.8) minimum | lb/in (N) | ASTM D5034, grab method |
| Tensile strength – fill | 105 (467.3) minimum | lb/in (N) | ASTM D5034, grab method |
| Thickness | 0.004–0.005 (0.102–0.127) | in (mm) | ASTM D1777 |
| pH | 4.5–7.0 | — | AATCC 81 |
| Extractable materials | 0.5 maximum | % | ASTM D2257, petroleum ether |