Permabond® 910FS Cyanoacrylate is a 100% reactive, methyl-based cyanoacrylate adhesive designed for rapid, high-strength bonding. As the original 100% methyl cyanoacrylate, this solvent-free, low-viscosity liquid cures incredibly fast at room temperature when pressed into a thin film. It is specifically engineered to provide exceptional adhesion to metals—such as steel, aluminum, brass, and stainless steel—while also effectively bonding a wide variety of plastics and rubbers.
Key features
- Extremely fast setting: Rapidly develops high strength without mixing or heat curing, achieving fixture times of under 5 seconds on steel.
- Excellent metal adhesion: Specially designed to provide superior bond strength (up to 4200 psi) on a variety of metal surfaces.
- Industry approved: Meets rigorous specifications, including approval to MIL-A-46050C Type I Class 1 for existing designs and CID A-A-3097 Type I Class 1 for new designs.
Applications / Suitable for
- High-strength bonding of metals, including steel, aluminum, and brass
- Bonding various plastics and rubbers
- High-speed assembly requiring rapid fixture times
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical Composition | Methyl cyanoacrylate | - | - |
| Appearance | Colorless | - | Liquid |
| Viscosity | 2-4 | cP | at 25°C (mPa.s) |
| Specific Gravity | 1.1 | - | - |
| Maximum Gap Fill | 0.05 | mm | (0.002 in) |
| Flash Point | 83 | °C | (181.4°F) |
After-processing / final-state properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Fixture/Handling Time | < 5 | seconds | Steel |
| Full Strength | 24 | hours | - |
| Shear Strength | 23-29 | N/mm² | Steel (ISO 4587) (3300-4200 psi) |
| Impact Strength | 3-5 | kJ/m² | ASTM D-950 (1.4-2.4 ft-lb/in²) |
| Hardness | 85 | Shore D | ISO 868 |
| Dielectric Constant | 2.5 | - | at 10kHz |
| Dielectric Strength | 25 | kV/mm | - |
| Coefficient of Thermal Expansion | 90E-6 | mm/m/°C | - |
| Coefficient of Thermal Conductivity | 0.1 | W/(m.K) | - |