PERMABOND 799
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

Main features
- Up to 0.5 mm Gap Fill
- 8-Second Fixture Time
- MIL-A-46050C Type II Class 3 Compliance
Product Description
Permabond® 799 Cyanoacrylate is a high-viscosity, surface-insensitive adhesive that combines extremely fast curing with the ability to fill large gaps up to 0.5 mm. This 100% reactive, solvent-free formula minimizes frosting and fogging during cure and is particularly well-suited for porous substrates, as it fixtures before wicking into surface pores. It delivers rapid, high-strength bonds on a variety of materials, including plastics, metals, ceramics, and elastomers.
Key features
- Extremely fast setting: Polymerizes rapidly to achieve handling strength in just 8 seconds on steel, rubber, and phenolic surfaces.
- High viscosity: Specifically formulated with a 5000 cP viscosity to cure through large gaps and excel on porous substrates without premature wicking.
- Industry approved: Approved to stringent military specifications, including MIL-A-46050C Type II Class 3 for existing designs.
Applications / Suitable for
- Bonding plastics, metals, ceramics, and elastomers
- Large gap filling applications up to 0.5 mm
- Porous substrates where adhesive wicking must be prevented
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical Composition | Ethyl cyanoacrylate | - | - |
| Appearance | Colorless | - | Liquid |
| Viscosity | 5000 | cP | at 25°C (mPa.s) |
| Specific Gravity | 1.1 | - | - |
| Maximum Gap Fill | 0.5 | mm | (0.02 in) |
| Flash Point | 80-93 | °C | (176°F - 199.94°F) |
| Volatile Organic Compound | < 3 | % | EC Directive 2004/42/EC |
After-processing / final-state properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Fixture/Handling Time | 8 | seconds | Steel, Buna N Rubber, Phenolic |
| Full Strength | 24 | hours | - |
| Shear Strength | 20-22 | N/mm² | Steel (ISO 4587) (2900-3200 psi) |
| Impact Strength | 3-5 | kJ/m² | ASTM D-950 (1.4-2.4 ft-lb/in²) |
| Hardness | 85 | Shore D | ISO 868 |
| Dielectric Constant | 2.5 | - | at 10kHz |
| Dielectric Strength | 25 | kV/mm | - |
| Coefficient of Thermal Expansion | 90E-6 | mm/mm/°C | - |
| Coefficient of Thermal Conductivity | 0.1 | W/(m.K) | - |