PERMABOND 101
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

Main features
- 2 to 3 mPa s Viscosity Range
- 2 to 10-Second Fixturing Time
- 25 kV/mm Dielectric Strength
Product Description
PERMABOND® 101 Cyanoacrylate Adhesive is an ultra-low-viscosity, single-component ethyl cyanoacrylate adhesive for wicking into close-fitting joints and bonding pre-assembled parts. It cures rapidly when confined as a thin film between surfaces, with typical handling strength reached in 2–10 seconds depending on the substrate. The adhesive is suitable for plastics, rubber, and metals and has a maximum recommended gap fill of 0.05 mm. After cure, it provides high shear strength on steel and other substrates, 85 Shore D hardness, and electrical insulation properties suitable for industrial assembly applications.
Key features
- Ultra-low viscosity: A 2–3 mPa·s viscosity supports capillary wicking into closely fitted and pre-assembled joints.
- Fast fixture time: Typical handling strength is achieved in 2–10 seconds, depending on the bonded substrate.
- Multi-material bonding: Supports bonding of plastics, rubber, and metals, with documented shear data on steel, aluminum, zinc, ABS, PVC, polycarbonate, and phenolic.
Applications / Suitable for
- Pre-assembled components
- Close-fitting plastic parts
- Wicking and penetrating applications
- High-speed industrial assembly
- Bonding plastics, rubber, and metals
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Typical uncured and curing properties. Values are guideline information and are not product specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical composition | Ethyl cyanoacrylate | — | Single-component adhesive |
| Appearance | Colorless liquid | — | As supplied |
| Viscosity | 2–3 | mPa·s | At 25 °C; equivalent to cP |
| Specific gravity | 1.1 | — | Typical uncured value |
| Maximum gap fill | 0.05 | mm | Equivalent source value 0.002 in |
| Fixture time — steel | 3–5 | s | Time to 0.3 N/mm² shear strength |
| Fixture time — Buna N rubber | 2–5 | s | Time to 0.3 N/mm² shear strength |
| Full strength | 24 | h | Typical full-strength development |
As-supplied / before-processing properties
Typical uncured and curing properties. Values are guideline information and are not product specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical composition | Ethyl cyanoacrylate | — | Single-component adhesive |
| Appearance | Colorless liquid | — | As supplied |
| Viscosity | 2–3 | mPa·s | At 25 °C; equivalent to cP |
| Specific gravity | 1.1 | — | Typical uncured value |
| Maximum gap fill | 0.05 | mm | Equivalent source value 0.002 in |
| Fixture time — steel | 3–5 | s | Time to 0.3 N/mm² shear strength |
| Fixture time — Buna N rubber | 2–5 | s | Time to 0.3 N/mm² shear strength |
| Full strength | 24 | h | Typical full-strength development |