LOCTITE SICOMET 100
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

Main features
- 0.01 to 0.50 mm Gap Fill
- Fast Moisture-Cure Fixturing
- Strong Rubber/Plastic Adhesion
Product Description
LOCTITE® SICOMET 100 is a fast-curing, medium-viscosity ethyl cyanoacrylate instant adhesive designed for bonding a wide range of materials including plastics, rubbers, metals, fabrics, and foam materials. The one-component adhesive cures rapidly through surface moisture and develops handling strength within seconds on close-fitting parts. It offers excellent adhesion to plastics and elastomers while requiring no mixing, making it suitable for high-speed assembly and repair operations.
Key Features & Benefits
- Ethyl cyanoacrylate instant adhesive technology.
- Excellent adhesion to rubbers and plastics.
- Fast fixture and cure speed.
- Medium-low viscosity for easy application.
- One-component formulation requiring no mixing.
- Easy dispensing and handling.
- Suitable for close-fitting assemblies.
Recommended Applications
- Plastic component assembly.
- Rubber and elastomer bonding.
- Foam material bonding.
- Metal bonding applications.
- Fabric assembly and repair.
- General-purpose instant bonding operations.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
As-Supplied / Before-Processing Properties
| Property | Value | Unit | Condition |
|---|---|---|---|
| Technology | Ethyl Cyanoacrylate | — | Instant adhesive |
| Appearance | Colourless Liquid | — | Uncured material |
| Components | One Part | — | No mixing required |
| Viscosity Classification | Medium-Low | — | Product characteristic |
| Specific Gravity | 1.05 - 1.10 | — | 25°C |
| Viscosity | 140 - 220 | mPa·s (cP) | 25°C |
| Cure Mechanism | Surface Moisture | — | Moisture activated |
After-Processing / Final-State Properties
| Property | Value | Unit | Condition / Method |
|---|---|---|---|
| Recommended Gap Fill | 0.01 - 0.50 | mm | Typical bond gap |
| Fixture Time (Aluminium) | 5 - 10 | seconds | Typical cure speed |
| Fixture Time (Steel) | 10 - 30 | seconds | Typical cure speed |
| Fixture Time (Rubber, Nitrile) | 5 - 10 | seconds | Typical cure speed |
| Fixture Time (ABS) | 5 - 10 | seconds | Typical cure speed |
| Fixture Time (PVC) | 5 - 10 | seconds | Typical cure speed |
| Tensile Shear Strength (Steel) | 17 | N/mm² | ISO 4587, 24 h cure |
| Tensile Shear Strength (Aluminum) | 15 | N/mm² | ISO 4587, 24 h cure |
| Tensile Shear Strength (ABS) | 8* | N/mm² | Substrate failure |