LOCTITE EA 9891RP

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EA 9891RP

Main features

  • Visual Color-Change Mix Verification
  • Room-Temperature Abradable Seal Repair
  • Abrasion-Resistant Paste Restoration

Product Description

LOCTITE EA 9891RP AERO is a two-component, room-temperature-curing epoxy repair paste for restoring LOCTITE EF 9890 AERO and SynSpand 9890 abradable seal materials. The abrasion-resistant paste is applied to localized worn or damaged areas, and a color-change mixing indicator confirms uniform blending of Parts A and B. The paste supports controlled placement on abradable surfaces, while room-temperature cure limits the need for elevated-temperature processing. Its application scope is the 9890 abradable-seal repair system and related paste repairs.

Key features

  • Visual mix confirmation: A color-change indicator helps confirm uniform blending of the two components.
  • Room-temperature repair cure: The epoxy paste cures at room temperature for localized repair processing.
  • Abrasion-resistant restoration: The repair paste restores LOCTITE EF 9890 AERO and SynSpand 9890 abradable seal materials.

Applications

Applications include repair of LOCTITE EF 9890 AERO and SynSpand 9890 abradable seal materials.

Product Family

LOCTITE EA 9891RP

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component SystemComponent System
Two (A / B)
Density (g)Density (g)
0.7 / 0.5 g/cm3
Mix RatioMix Ratio
100: 40
Pot LifePot Life
20 minutes minutes

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers