U-847 | Dimer Diisocyanate Urethane Dimethacrylate
Harmonization Code : 3909.50 | Amino-resins, phenolic resins and polyurethanes, in primary forms

Main features
- Low color
- Low cure shrinkage
- BPA-free
Product Description
DMI U-847 is a high-purity, methacrylate-modified urethane monomer designed for use in advanced light-cure formulations, particularly within the dental industry. Its low color and low polymerization shrinkage properties make it especially suitable for aesthetic and precision applications where dimensional stability is critical.
Unlike BisGMA or other Bisphenol A-based materials, DMI U-847 is engineered without a BPA backbone, eliminating the risk of estrogenic behavior or endocrine disruption. This makes it a safe and reliable choice for health-conscious formulations in dental, medical, and other regulated industries.
Applications
- Light-cure dental adhesives, composites, and sealants
- Medical-grade formulations requiring BPA-free materials
- Base resin in photopolymer systems where low shrinkage and high clarity are essential
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
Molecular Formula: C50H90N2O8
CAS Registration Number: 86499-57-3
Recommended Formulation Use
U-847 is recommended for use as a base resin in dental applications.