A1050 | Anti bleed Additive

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

A1050 | Anti bleed Additive

Main features

  • Silver filled systems
  • 100 mPa-s Viscosity
  • Non halogenated

Product Description

A-1050 (Part number A-6150) is a proprietary non-halogenated additive designed to reduce resin bleed out on a variety of surfaces with minimal or no affect on the adhesion properties of the formulation. It shows excellent results when used with metal filler systems such as silver. It also shows improved bleed properties with non-metal filled systems. It is co-curable in free-radical polymerization. It also can enhance the rheological properties of various filled adhesives.dhesives.

A-1050 is recommended for use as an additive to reduce resin bleed out specifically on metal surfaces. The recommended addition of the A-1050 to a formulation is between 0.5% - 1% weight percent of resin. It shows superior bleed control in silver filled formulations and can significantly reduce or eliminate resin bleed out in formulations that contain non-metal fillers such as silica. The addition of the A-1050 has also shown to significantly increase the thixotropic nature of silver filled adhesives.

Product Family

DMI A1050

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US No longer available
CA No longer available
EU Shipping in 2 weeks
TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Yellow liquid
Density (g)Density (g)
0.98 g/cm3
FunctionalityFunctionality
1 Functional group/molecule
Molecular weightMolecular weight
1113 (estimated) g/mol
Thermal Properties
Flash PointFlash Point
200 °C
Physical Properties
ViscosityViscosity
100 mPa.s

Additional Information

A1050 Vs A1100 (Parts #A6150 vs #A6265)

A1050 and A1100 are similar in that they have acid functionality and are both good for metal surfaces. Of the two A1050 has been used successfully by industry leading sealant companies and is now used by major conductive die attach paste manufacturers.
A1050 has a more extensive track record while A1100 is a similar and potentially better alternative that is currently implemented in new processes.

Epoxy Resin Incompatibility

A1050 rely on acid functionality to bond in and prevent bleeding. Unfortunately thiol group react with epoxy resin instead of substrate reducing or even eliminating the resin bleed functionality.

Molecular Weight Estimation

We do not specifically measure the M.W. for this material and instead rely on the average M.W. of the starting material and the functionality (thiol group) that makes the product.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers