Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

Main features
- One-Month Mixed Working Life
- 17.8 to 25.4 um Film
- Spray, Brush or Dip Application
Product Description
Chemlok 485 / Curative 44 Adhesive System is a two-component insert-molding adhesive system for bonding supported PVC and Alcryn-type thermoplastic elastomers to metal and rubber substrates. The system is prepared by adding 6 to 10 parts Curative 44 by weight to 100 parts Chemlok 485. When sealed from moisture at room temperature, the mixed material has an approximate working life of one month. It can be applied by spray, brush, or dip, with a recommended dry film thickness of 17.8 to 25.4 um before molding. The system is intended for supported insert-molding applications using the documented surface preparation and drying process.
Key features
- Controlled Two-Component Mix: mix 100 parts Chemlok 485 with 6 to 10 parts Curative 44 by weight
- Extended Mixed Working Life: mixed material has an approximate one-month working life at room temperature when sealed from moisture
- Defined Dry Film: recommended dry film thickness is 17.8 to 25.4 um before molding
Applications
Insert molding of supported PVC and Alcryn-type thermoplastic elastomers to metal and rubber substrates.
Technical Specifications
Physical Properties
General Properties
Additional Information
As-supplied / before-processing properties
Component properties and mixed-system handling values are identified separately.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemlok 485 viscosity | 400 to 1000 | cps | 25 deg C; Brookfield LVT, spindle 2, 30 rpm; typical |
| Curative 44 viscosity | Less than 10 | cps | 25 deg C; typical |
| Chemlok 485 density | 850.8 to 874.7 | kg/m^3 | Typical |
| Curative 44 density | 1010 to 1040 | kg/m^3 | Typical |
| Chemlok 485 solids by weight | 15 to 17 | % | Typical |
| Curative 44 solids by weight | 47 to 51.5 | % | Typical |
| Mix ratio | 100 : 6 to 10 | parts by weight | Chemlok 485 : Curative 44 |
| Mixed working life | Approximately 1 | month | Room temperature; sealed from moisture |