BONDERITE L-GP-D148A
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- PTFE Dry-Film Lubricant Formation
- Spray-Viscosity Thinning Compatibility
- Room-Temperature Cure with Heat Acceleration
Product Description
BONDERITE L-GP D 148A is the PTFE-based varnish component of a two-part dry-film lubricant system. It is combined with the separately supplied BONDERITE S-OT Durcisseur hardener, and the blended resin and hardener are adjusted to spray viscosity using thinner. After application, the mixed system cures at room temperature in approximately 24 hours to form a smooth, dry, PTFE-lubricating film; heat can be used to accelerate the cure. Because this product is one component of a matched two-part system, its final coating performance depends on correct combination and cure with the BONDERITE S-OT Durcisseur hardener as directed in the manufacturer's technical documentation.
Key features
- PTFE Dry-Film Lubricant Chemistry: PTFE-based varnish that develops a dry, lubricating coating after curing
- Two-Component System with S-OT Durcisseur: requires the separately supplied BONDERITE S-OT Durcisseur hardener as a matched two-part system
- Spray-Viscosity Thinning and Room-Temperature Cure: blend is adjusted to spray viscosity with thinner and cures in about 24 hours at room temperature, with heat-accelerated options
Applications
Applications include dry-film lubrication of metal components after the product is mixed and cured with the BONDERITE S-OT Durcisseur hardener.