BONDERITE C-IC DEOXIDOZER
Harmonization Code : 3810.10.00 | Soldering, brazing or welding powders and pastes consisting of metal and other materials

Main features
- Aluminum Deoxidizing, Desmutting, Etching
- Prepares for Chromating
- 1 to 10 Minute Application Rate
Product Description
BONDERITE C-IC DEOXDZR 6 MU is a liquid metal pretreatment additive used with mineral-acid immersion baths for deoxidizing, desmutting, and etching aluminum. The system supports aluminum surface preparation before chromating or anodic coloring and can also be used for etching before thermal welding.
Key features
- Acid-bath aluminum pretreatment: Used with nitric acid or sulfuric acid immersion baths for deoxidizing, desmutting, and etching aluminum.
- Multiple downstream processes: Supports aluminum preparation before chromating, anodic coloring, or thermal welding.
- Controlled immersion treatment: Recommended working parameters include 5% v/v product concentration, 20 to 30°C bath temperature, and 1 to 10 minutes treatment time.
Applications / Suitable for
- Deoxidizing and desmutting aluminum before chromating
- Pretreatment of aluminum before anodic coloring
- Aluminum etching before thermal welding
TDS, SDS & Technical Documents
Technical Specifications
No specifications available.
Additional Information
Technical properties
As-supplied / before-processing properties
Properties apply to BONDERITE C-IC DEOXDZR 6 MU before addition to the working bath.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Physical form | Liquid additive | — | As supplied |
| Recommended storage temperature | -20 to +50 | °C | Recommended storage range |
| Shelf life | 36 | months | Unopened original packaging at the recommended storage temperature |