BONDERITE C-AD 4215

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-AD 4215

Main features

    Product Description

    BONDERITE® C-AD 4215 AERO is a clear, colorless liquid additive formulated to enhance the cleaning performance of BONDERITE® C-AK 4215 AERO and other alkaline cleaners when difficult-to-remove soils are encountered. Suitable for both spray and immersion cleaning systems, the additive readily dissolves into alkaline cleaning baths, is compatible with ferrous and nonferrous alloys when used with a compatible base cleaner, and rinses cleanly from treated parts with cool to warm water.

    Key Features

    • Cleaning-performance enhancer for BONDERITE® C-AK 4215 AERO and other compatible alkaline cleaners.
    • Low addition rate of only 1–2% by volume minimizes changes to existing cleaning processes.
    • Suitable for spray and immersion systems with recommended air or mechanical agitation for immersion cleaning.
    • Compatible with ferrous and nonferrous alloys when the selected alkaline cleaner is also compatible.
    • Readily soluble and free-rinsing for efficient incorporation into alkaline cleaning baths.

    Applications / Suitable for

    • Enhancing alkaline cleaner performance
    • Spray alkaline cleaning systems
    • Immersion alkaline cleaning systems
    • Cleaning difficult-to-remove soils
    • Ferrous alloy cleaning processes
    • Nonferrous alloy cleaning processes
    Product Family

    BONDERITE C-AD 4215

    Catalog Product

    Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

    TDS, SDS & Technical Documents

    Technical Specifications

    Other Properties
    Storage TemperatureStorage Temperature
    0–40°C °C
    General Properties
    AppearanceAppearance
    Clear, colorless liquid
    Specific GravitySpecific Gravity
    Density: 0.951–0.961 g/mL

    Additional Information

    Technical Properties

    As-Supplied / Before-Processing Properties

    Supplier-published characteristics of BONDERITE® C-AD 4215 AERO.

    Property Value Unit Method / Condition
    Technology Metal Pretreatment Supplier classification
    Product Type Additive Supplier classification
    Application Immersion and Spray Supplier classification
    Appearance Clear, colorless liquid As supplied
    Density 0.951–0.961 g/mL Typical property
    Flash Point 110 °C Cleveland Open Cup Method
    Storage Temperature 0–40 °C Recommended storage
    Shelf Life 24 months Original unopened packaging
    Technical Properties

    After-Processing / Operating Properties

    Supplier-recommended operating conditions when using BONDERITE® C-AD 4215 AERO with compatible alkaline cleaners.

    Property Value Unit Method / Condition
    Recommended addition level 1–2 % by volume Add after alkaline cleaner is fully mixed
    Operating temperature 60–80 °C Preferred operating range
    Preferred operating temperature 70 °C Supplier recommendation
    Application methods Spray and immersion Compatible alkaline cleaning systems
    Immersion agitation Air or mechanical agitation recommended Immersion cleaning
    Rinsing Cool to warm water rinse Follow rinsing procedure of the selected alkaline cleaner
    Compatibility Ferrous and nonferrous alloys Provided the base cleaner is compatible with the substrate

    Leading Brands Trust in Our Products and Services

    • Jabil
    • Linxens
    • Magna
    • Medtronic
    • NXP
    • Philips
    • Semikron
    • Teledyne
    • Thales
    • Vishay
    • ZF
    • AMS
    • Apple
    • Audi
    • Broadcom
    • Borgwarner
    • Bosch
    • Eaton
    • Henkel
    • Honeywell
    • Hysol
    • Intel
    Products that Perform|Knowledge that Serves|Service that Delivers