ARALDITE AW139
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- Two-Component Room-Temperature Epoxy
- High-Temperature Chemical Resistance
- Multi-Material Metal/Composite/Electronics Bonding
Product Description
ARALDITE® AW 139-1 / Hardener HW 5323-1 is a two-component, room-temperature-curing epoxy paste adhesive for structural bonding where elevated temperatures or aggressive service environments may be encountered. The thixotropic, non-sagging mixed adhesive fills gaps up to 5 mm and is suitable for bonding metals, electronic components, GRP structures, and other supported assemblies. A 100:50 mix ratio by weight or volume, approximately 110-minute pot life at 25°C, and specified lap shear strength above 14 MPa at 25°C provide a practical balance of application control and bonded-joint performance.
Key features
- Environmental resistance: Resistant to water and a wide variety of chemicals.
- Gap-filling paste: Thixotropic, non-sagging consistency supports gaps up to 5 mm.
- Controlled working time: Approximately 110-minute pot life for a 100 g mixed mass at 25°C.
Applications / Suitable for
- Structural bonding of metals
- Bonding electronic components
- GRP structures and assemblies exposed to demanding environments
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Electrical Properties
Additional Information
Before-mixing properties
Individual component properties before ARALDITE® AW 139-1 and Hardener HW 5323-1 are combined.
| Property | ARALDITE® AW 139-1 | Hardener HW 5323-1 |
|---|---|---|
| Color and form | Beige paste | Grey paste |
| Specific gravity | Approx. 1.6 | Approx. 1.5 |
| Viscosity at 25°C | 50–80 Pa·s | Thixotropic |
| Mix ratio | 100 parts AW 139-1 to 50 parts HW 5323-1 by weight or volume | |
After-mixing properties
Properties of the mixed adhesive before cure.
| Property | Value | Condition |
|---|---|---|
| Color and form | Grey paste | Mixed adhesive |
| Specific gravity | Approx. 1.6 | Mixed adhesive |
| Rheology | Thixotropic | Non-sagging paste |
| Pot life | 110 minutes | 100 g mixed mass at 25°C |
| Gap-filling capability | Up to 5 mm | Non-sag application |