Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M™ Scotch-Weld™ Epoxy Adhesive DP110

Main features

  • Controlled flow
  • 20-minute handling strength
  • Good adhesion to many plastics and metals

Product Description

3M™Scotch-Weld™ Epoxy Adhesive DP110 is a flexible, fast-curing, two-part structural epoxy. It provides excellent shear and peel strength while remaining highly adaptable to thermal expansion and vibration.

Product Key Features

  • Controlled flow
  • 20 minute handling strength
  • Duo-Pak cartridge dispensing system
  • Good adhesion to many plastics and metals

Applications

  • Signage & Display Assembly: Bonding plastic lettering or transparent panels to metal frames with invisible seams.
  • Sporting Goods Manufacturing: Assembling composite, metal, or fiberglass parts that require high impact resistance.
  • General Industrial Bonding: Joining dissimilar substrates (like aluminum to plastic) prone to thermal movement.
  • Electronic Component Encapsulation: Securing parts and sealing joints against moisture without high visual opacity.
Product Family

3M DP110

1. Select Package Type
2. Select Color
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 2 weeks
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry TypeChemistry Type
Modified Epoxy
ColorColor
Yellow Translucent
Mix RatioMix Ratio
1:1

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers