Optical sensors are primarily separated into through hole, surface mount and map molded surface mount devices and are used for light sensing and data transmission.
Optoelectronic molding compound requirements.
Data transmission sensors need to operate on the 680nm wavelength range while light sensors should be able to operate either on the visible light spectrum (400-700nm) or on the infrared range (800-1500nm)
When it comes to package types, Through hole doesn't require MSL and the CTE is less important. Surface mount requires a certain MSL level while CTE is still not as important. And finally Map molded surface mount where both MSL needs to be attainable while CTE needs to be fine tuned to the substrate so that we avoid shrinkage and warpage.
For Through hole devices, there are some products that are "tried and true" and have proven their value in the industry. TC 8020T comes as a breakthrough product with better moldability, lower moisture absorption, better MSL level and heat resistance. On top of that, the adhesion to Cu is better than the main competitive choices.
|
|
Units |
XX324H-11000 |
XX18 |
KRAYDEN |
|
Specific Gravity |
g/cc |
1.25 |
1.33 |
1.23 |
|
Spiral Flow @ 150°C |
inches |
82 |
37 |
78 |
|
Hot Plate Gel Time @ 160°C |
seconds |
30 |
45 |
30 |
|
Cure Conditions |
4min@150°C |
4min@150°C + 3hr@150°C |
4min@150°C + 3hr@150°C |
|
|
Hardness |
Shore D |
86 |
85 |
86 |
|
Mold Shrinkage |
% |
1.6 |
1.6 |
1.6 |
|
Tg by TMA |
°C |
130 |
125 |
125 |
|
CTE by TMA, Alpha1 CTE by TMA, Alpha2 |
ppm/°C |
65 |
70 |
70 |
|
Moisture absorption 24hrs @ 25°C |
|
|
0.77 |
0.32 0.17 |
|
Flexural Strength @25°C Flexural Modulus @25°C |
MPa Gpa |
129 |
107 |
130 |
|
Refractive Index @633nm |
- |
1.57 |
1.52 |
1.56 |
|
Transmittance @460nm, initial |
% |
>90% |
>90% |
> 90% |
|
after 10,000 hrs @ 125°C |
% |
83% |
72% |
86% |
|
after 1,000 hrs @ 150°C |
63% |
27% |
68% |
|
|
MSL JEDEC Level Capable |
- |
MSL 4 |
MSL 4 |
MSL 3 |
Die attach Requirements
- Application by printing, dispensing, jetting & pin transfer
- High adhesion on LCP & metal finishes
- Low outgassing