MOLYKOTE G2008
Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

Main features
- High-Speed Gear Lubrication
- 30 cSt Synthetic Base Oil
- -40 to 130 deg C Service
Product Description
MOLYKOTE G-2008 Synthetic Tool & Gear Grease is a dark-gray PAO/lithium grease with solid lubricants for high-speed gears and high-shear mechanical contacts. The NLGI 2 formulation uses a 30 cSt base oil at 40 deg C and operates from -40 to 130 deg C. It is applied through conventional grease methods, including brush, grease gun, and manual or automated dispensing. Primary uses include planetary, worm, spur, and helical gears in power tools and drills, plus cables, gears, and selected bearings exposed to high shear.
Key features
- High-Speed Gear Lubrication: The formulation is intended for planetary, worm, spur, and helical gears in compatible power tools and drills.
- 30 cSt Synthetic Base Oil: A fully synthetic PAO base oil provides low-viscosity flow at 40 deg C.
- Controlled Bleed and Evaporation: Typical 24-hour results at 100 deg C are below 5.0 wt% oil bleed and below 1.0 wt% evaporation.
Applications / Suitable for
- Planetary, worm, spur, and helical gears.
- Compatible power tools and drills.
- High-shear cables, gears, and selected bearings.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied grease properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| NLGI consistency | 2 | Typical | |
| Worked penetration | 260 to 300 | mm/10 | ASTM D217 at 25 deg C, W/60; typical |
| Base-oil viscosity | 30 | cSt | ASTM D445 at 40 deg C; typical |
| Dropping point | >200 | deg C | ASTM D2265; test result, not a service-temperature limit |
| Usable life | 18 | months | Original unopened container stored at or below 40 deg C |
In-service performance properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Service-temperature range | -40 to 130 | deg C | Supplier product page |
| Four-ball wear scar | <0.55 | mm | ASTM D2266, 40 kg, 1,200 rpm, 1 h at 75 deg C; typical |
| Oil bleed | <5.0 | wt% | CTM 0033A at 100 deg C for 24 h; typical |
| Oil evaporation | <1.0 | wt% | CTM 0033A at 100 deg C for 24 h; typical |