MOLYKOTE G-4501

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE G-4501

Main features

  • FDA 21 CFR 178.3570 Compliance
  • Lower-Consistency (NLGI 1) PAO Synthetic Grease
  • 40 to 150 deg C Service Range

Product Description

MOLYKOTE® G-4501 FM Multi-Purpose Synthetic Grease is a high-performance, food-grade lubricant formulated with a polyalphaolefin (PAO) synthetic base oil, an aluminum complex thickener, and fortified with polytetrafluoroethylene (PTFE). Designed as an NLGI 1 grease, its lower consistency makes it highly suitable for use in automatic dispensing systems. It delivers greater wear resistance, higher load-carrying capacity, and longer service life compared to conventional petroleum-based lubricants.

Key features

  • Food-grade compliance: Meets FDA Regulation 21 CFR 178.3570 and USDA H1 classifications for safe use in incidental food contact applications.
  • Broad material compatibility: Highly compatible with most industrial and engineering substrates, including a wide variety of plastic and rubber materials.
  • Wide temperature capability: Provides excellent low-temperature torque and reliable performance across a broad service temperature range of -40°C to 150°C (-40°F to 302°F).

Applications / Suitable for

  • Food processing machinery requiring incidental food contact lubricants
  • Rolling element and plain bearings
  • Pivot pins, cams, guides, ways, drive screws, gears, and splines
  • Automatic grease dispensing systems

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition PAO base oil, aluminum complex thickener, PTFE - Organic grease containing white mineral oil
Appearance / Color White / Off-white - Grease
NLGI Consistency Class 1 - DIN 51 818
Worked Penetration 310 - 340 mm/10 at 25°C (77°F) (W/60) (ASTM D217)
Base Oil Viscosity (40°C) 100 cSt at 40°C (104°F) (ASTM D445)
Base Oil Viscosity (100°C) 14.4 cSt at 100°C (212°F) (ASTM D445)
Specific Gravity / Relative Density 0.83 g/ml at 25°C (77°F) (ISO 2811)
Flash Point > 200 °C Closed cup (> 392°F)
Shelf Life 60 months From the date of production when stored at or below 40°C (104°F) in unopened containers
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Service Temperature Range -40 to 150 °C (-40 to 302°F) Approximate
Dropping Point > 260 °C (> 500°F) (ASTM D2265)
Low-Temperature Torque 0.7 Nm at -40°C (-40°F) (ASTM D4693)
Four-Ball Wear Scar 0.5 mm 40 kg, 1,200 rpm (ASTM D2266)
Four-Ball EP Weld Load > 3,100 N Minimum (ASTM D2596)
TIMKEN OK Load > 18 kg ASTM D2509
Dn Value 325,000 mm/min Estimated (bearing ID x rpm)
Oil Bleed 4.7 wt% 24 hours at 100°C (212°F) (FD 791-32/2)
Oil Evaporation 0.5 wt% 24 hours at 100°C (212°F) (FD 791-32/2)

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers