MOLYKOTE G-0052
Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

Main features
- FDA 21 CFR 178.3570 Compliance
- 6,080 N Four-Ball Weld Load
- Water-Resistant Grease Lubrication
Product Description
MOLYKOTE® G-0052 FM White E.P. Bearing Grease is a high-performance, mineral-oil-based lubricant thickened with an aluminum complex. Specially formulated for the food and beverage industry, this white, NLGI 2 multipurpose grease is fortified with extreme pressure (EP) and anti-wear (AW) additives to protect highly loaded mechanical components. It provides an excellent lubrication solution where an NSF H1 status lubricant is required or when the environment must remain free of black particle contamination.
Key features
- Food-grade compliance: Meets FDA Regulation 21 CFR 178.3570, holds the NSF H1 classification for incidental food contact, and is Kosher approved.
- High load capacity: Effectively protects bearings and gears under heavy loads, demonstrating a high four-ball weld load of 6,080 N (620 KG).
- Robust environmental resistance: Provides good resistance to water washout and is broadly compatible with many plastics and elastomers used in food processing machinery.
Applications / Suitable for
- Multipurpose lubrication of mechanical components in food and beverage processing facilities
- Anti-friction bearings and plain bearings
- Chains, gears, and sliding mechanisms
TDS, SDS & Technical Documents
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical Composition | Mineral oil, aluminum complex thickener, EP/AW additives | - | Contains zinc oxide |
| Appearance / Color | White | - | Grease |
| NLGI Consistency Class | 2 | - | DIN 51 818 |
| Penetration | 280 | mm/10 | ASTM D217 |
| Density | 0.89 - 1.08 | g/ml | at 20°C (ISO 2811). |
| Base Oil Viscosity | 99 | cSt | at 40°C (ASTM D445) |
| Flash Point | > 200 | °C | Closed cup |
| Usable Life | 60 | months | From date of production when stored at or below 32°C (90°F) in unopened containers |
After-processing / in-service properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Service Temperature Range | -17 to +150 | °C | (0 to +302 °F) |
| Drop Point | 269 | °C | (516 °F) (ASTM D2265) |
| Four-Ball Weld Load | 6,080 | N | (620 KG) (ASTM D2596) |
| Four-Ball Wear Scar | 0.9 | mm | ASTM D2266 |
| Water Washout | 10 | % | at 175°F (ASTM D1264) |
| Oil Bleed | <= 5 | % max | 24 hrs @ 100°C (Fed 791) |
| Oil Evaporation | <= 2.0 | % max | 24 hrs @ 100°C (Fed 791) |