LOCTITE LF 318

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

LOCTITE LF 318

Main features

  • 90iSC Alloy
  • Automotive reliability qualified
  • Stencil Printable

Product Description

LOCTITE LF 318 solder paste is a halide-free, no clean, pin testable Pb-free solder paste, formulated to have excellent humidity resistance and a broad process window, both for reflow and printing. This product has high tack force to resist component movement during high speed placement and long printer abandon times.

LOCTITE LF 318 shows excellent solderability over a wide range of reflow profiles in both air and nitrogen across a wide range of surface finishes including Ni/Au, Immersion Sn, Immersion Ag, OSP copper. It leaves colorless and soft, non stick residues for easy post reflow inspection and in-circuit testing.

LOCTITE LF 318 should not be used to solder to component or PCB finishes containing lead (Pb), as a low melting eutectic (at 98°C) will form. It is suitable for fine pitch, high speed printing and pneumatic dispensing.

LOCTITE LF 318 contains a modified Pb-free solder alloy developed in a co-operative project for improved reliability as compared with standard SAC alloys, with a standard flux medium , LF 318.

Product Family

LOCTITE LF318

No longer available

This product is no longer available from Krayden. Please contact us so we can recommend an alternative product.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy TypeAlloy Type
90iSC
Physical Properties
Thixotropic indexThixotropic index
0.5
ViscosityViscosity
650,000 mPa.s

Additional Information

Solder Alloys (J-STD 006)

Code Allloy Melting point Ag%
SAC0307 Low Silver 217 to 226 0.3
90iSC High Reliability 205 to 218 3.8
96S Industry Standard 221 3.5
96SC Industry Standard 217 3.8
97SC Industry Standard 217 3.0

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers