LOCTITE D125 F

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE D125 F

Main features

  • Low exotherm
  • High speed dispensing
  • Low cure temperature

Product Description

LOCTITE D 125 F is a one-component, heat-curable epoxy adhesive specifically formulated for high-speed dispensing in surface mount technology (SMT) assembly. With its low exotherm and minimal water absorption, LOCTITE D 125 F reduces thermal stress on components while ensuring strong adhesion and process reliability.

This yellow adhesive exhibits excellent non-sag and non-stringing characteristics, enabling precise, clean application for chip capacitors, chip resistors, SOTs, SOICs, and PLCCs. It offers high hot strength and fast curing at low temperatures, making it well-suited for demanding, high-throughput electronic manufacturing.

Applications

  • Surface mount assembly of chip capacitors and resistors
  • Bonding SOTs, SOICs, PLCCs, and other SMT components
  • High-speed, precision dispensing processes
  • Electronics production requiring low cure temperatures and non-sag adhesives
Product Family

LOCTITE D125

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 25 days
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific GravitySpecific Gravity
1.275
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
85 °C
Thermal ConductivityThermal Conductivity
0.3 W/m.K
Electrical Properties
Volume ResistivityVolume Resistivity
1e 14 Ohms⋅cm
Physical Properties
ViscosityViscosity
1750000 mPa.s

Additional Information

Cure Profiles
IR or Convection Conveyor Oven:

  • 20 min @ 100 °C

  • 7 min @ 110 °C

  • 2.5 min @ 120 °C

  • 1.5 min @ 150 °C

Convection Box Oven:

  • 30 min @ 100 °C

  • 20 min @ 110 °C

  • 10 min @ 120 °C

  • 5 min @ 150 °C

*Note: Ramp-up should not exceed 1 °C per second

Thawing

  1. Remove the adhesive from cold storage.

  2. Allow the material to reach room temperature (25 °C) before use.

  3. Do not re-freeze once thawed.

  4. Once thawed, apply using the recommended methods.

Directions for Use

  1.  LOCTITE D125 F can be applied by dispensing, pin transfer, screen or stencil printing.
  2. Equipment set-up and related product information is available from your Henkel Corporation support group.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers