LOCTITE 3616
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Main features
- One component
- High wet strength
- SMD to PCB adhesive
Product Description
LOCTITE 3616 is a "chipbonder" designed for the bonding of surface mounted devices to printed circuit boards prior to wave soldering. Particularly suited to printing a range of dot heights with one stencil thickness and where high wet strength characteristics, and high print speeds are required.
LOCTITE 3616 is a heat curable and stencil printable, red, viscous, surface mount adhesive that is commonly used to attach small parts and SMD components on PCB.
Cure Schedule
- Recommended conditions for curing are exposure to heat above 100 °C (typically 90-120 seconds @ 150 °C).
- Rate of cure and final strength will depend on the residence time at the cure temperature.