LOCTITE 3217

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 3217

Main features

  • UV & Heat Cure
  • Non Conductive
  • Image sensor module assemblies

Product Description

LOCTITE 3217 dual cure adhesive is designed for use in the assembly of temperature sensitive electronic components. The maximum performance of this material is achieved by exposure to UV light of sufficient intensity, followed by thermal cure.

LOCTITE 3217 dual cure epoxy/acrylate (UV and heat) is an amber high viscosity material that is used for optical applications and the cavity fill of test IC's. It has good adhesion on glass and metals, based on customer experiences and it has been successfully used for Automotive applications.

 

UV Cure

  • Medium pressure mercury lamp UV Wavelength, nm 220 to 260
  • Light Intensity, mW/cm² 100
  • UV Tack-Free Time, seconds 1

Heat Cure

  • 30 minutes @ 60°C
  • 25 minutes @ 70°C
  • 20 minutes @ 80°C
Product Family

LOCTITE 3217

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 53 days
CA Shipping in 12 weeks
EU Shipping in 45 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot LifePot Life
336 hours
Specific GravitySpecific Gravity
1.2
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
82 °C
Physical Properties
Thixotropic indexThixotropic index
2.9
ViscosityViscosity
109,000 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers