LOCTITE 190017
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- Anaerobic Adhesive Technology
- Above 100 deg C Flash Point
- Clear Liquid Formulation
Product Description
LOCTITE 190017 1L EN is a clear, liquid anaerobic adhesive formulated for bonding and locking applications where curing occurs in the absence of air between closely fitting metal surfaces. The product exhibits a mild acrylic odor, a density of approximately 1.23 g/cm³, and a flash point greater than 100°C. Its liquid consistency supports dispensing and application in threaded assembly and retaining operations where anaerobic adhesive technology is commonly used. The material is supplied as a clear liquid and remains stable under recommended storage conditions. It is classified as a skin sensitizer and should be handled using appropriate industrial hygiene and personal-protection practices.
Key features
- Anaerobic adhesive technology: Designed to cure in the absence of air for locking and bonding applications.
- High flash point: Flash point greater than 100°C supports safer handling compared with lower-flash-point materials.
- Clear liquid formulation: Liquid delivery form supports controlled dispensing during assembly operations.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Physical properties of LOCTITE 190017 1L EN in its supplied liquid state.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Technology | Anaerobic adhesive | — | Product classification |
| Appearance | Clear liquid | — | Delivery form |
| Density | 1.2301 | g/cm³ | 20°C |
| Flash point | >100 | °C | Tagliabue closed cup |
| Kinematic viscosity | >20.5 | mm²/s | 40°C |
| Initial boiling point | >150 | °C | Physical property |