LINQSOL EMC-G833R | Black Epoxy Mold Compound
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Main features
- Green epoxy molding compound
- Designed for Quad Flat No Leads(QFN) and Quad Flat (QFP) packages
- Excellent reliability performance (MSL 1)
Product Description
LINQSOL™ EMC-G833R is a black, halogen-free (“green”) epoxy molding compound engineered for QFN, QFP, and other SMD packages. A long gel time (~52 s @ 175 °C) pairs with high spiral flow (~150 cm @ 175 °C) to deliver a generous processing window—ideal for thin runners, complex gate designs, and high-cavity tools typical of QFN/QFP molding. The compound’s low moisture uptake (~0.28% PCT-24 h) and very low ionic extractables (Cl⁻/Na⁺ ≈ 5 ppm) support MSL 1 capability, while UL-94 V-0 helps meet safety and compliance needs.
With a low CTE (α1 ≈ 10 ppm/°C, α2 ≈ 36 ppm/°C), low mold shrinkage (~0.15%), and balanced mechanicals (≈162 MPa flexural strength; ≈24 GPa modulus at 25 °C), EMC-G833R maintains dimensional control and package reliability through assembly and reflow. Recommended molding parameters (170–180 °C; 8–25 s transfer; 100–180 s cure @ 175 °C; post-mold cure 4–8 h @ 175 °C) fit standard transfer molding lines. Formulated RoHS & REACH compliant, EMC-G833R brings a dependable blend of throughput, yield, and long-term performance. EMC-G833R guarantees excellent performance and outstanding reliability. This product is deliberately formulated without the inclusion of substances prohibited by the European Union RoHS and REACH.
Overall, LINQSOL EMC-G833R seamlessly integrates advanced material properties, safety compliance, and superior performance to deliver a reliable solution for semiconductor device encapsulation.
Key Features
- High spiral flow (~150 cm @ 175 °C) — Fills fine-pitch and thin-gate QFN/QFP tools cleanly to reduce short-shots and voids.
- Long gel time (~52 s @ 175 °C) — Wide process latitude for complex runners and multi-cavity molds; easier parameter tuning.
- MSL 1 capable — Supports robust board-level reliability and simplified dry-pack handling.
- Ultra-low moisture & ions — ~0.28% (PCT-24 h) and Cl⁻/Na⁺ ≈ 5 ppm each help minimize popcorn, CAF, and leakage risk.
- Low CTE & shrinkage — α1 ≈ 10 ppm/°C, α2 ≈ 36 ppm/°C, shrinkage ~0.15% for coplanarity and warpage control.
- UL-94 V-0 — Meets stringent flammability requirements for safety-critical designs.
- Halogen-free (“Green”) — RoHS & REACH compliant formulation for global compliance.
Application Suitable for
- QFN families: QFN, DFN, MLF, QFNs with exposed pad / thermal slug
- QFP families: LQFP, TQFP, PQFP, thin-pack QFP variants
- Other SMD packages: SOP/SSOP/TSSOP/MSOP, small discretes requiring high flow and low warpage
- Use cases: High-cavity, fine-pitch transfer molding; assemblies needing MSL 1, low warpage, and UL-94 V-0 compliance
Technical Specifications
General Properties
Thermal Properties
Chemical Properties
Physical Properties
Mechanical Properties
Curing Conditions
Additional Information
LINQSOL EMC-G833 Series Product Property Comparison
| PROPERTY | UNIT | EMC-G833 | EMC-G833R |
|
Color |
– |
Black |
Black |
|
Filler content |
% |
87 |
88 |
|
Filler cut size |
µm |
75 |
75 |
|
Specific gravity |
– |
1.97 |
2.0 |
|
Spiral flow at 175 °C |
cm |
165 |
150 |
|
Ion content Chloride (Cl–) concentration Sodium (Na+) concentration |
ppm |
6 |
5 5 |
|
Electrical conductivity of extract |
µS⋅cm–1 |
50 |
30 |
|
Flexural strength |
MPa |
145 |
162 |
|
Flexural modulus |
GPa |
22.8 |
24 |
|
Glass transition temperature |
°C |
112 |
118 |
|
Coefficient of thermal expansion, α1 |
ppm/K |
11 |
10 |
|
Coefficient of thermal expansion, α2 |
ppm/K |
36 |
36 |
|
Gel time at 175 °C |
sec |
57 |
52 |
|
Flammability |
UL-94 |
V-0 |
V-0 |
LINQSOL EMC-G833R Storage and Handling
LINQSOL EMC-G833R is available in pressed pellets in a wide range of sizes to meet specific customer needs. To ensure product integrity, keep it away from oxidizing materials. For long-term storage, maintain a cold environment. The shelf life when stored below 5 °C is 183 days.
Please note that the provided information is based on available data and typical conditions. For specific applications and detailed test results, refer to the actual test data and conduct appropriate certifications.