PIT0.5S-DCD | 0.5 mil Die Cut Polyimide (Kapton) Tape with silicone adhesive| Single Sided Discs
Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

Main features
- 0.5 mil polyimide film
- Silicone Adhesive
- Die cut discs
Product Description
LINQTAPE PIT0.5S-DCD is a 0.5-mil, ultra thin Kapton HN Film with Silicone adhesive whose high performance, flexible, high-temperature resistant polyimide films are used for many demading applications. Polyimide is preferred over polyester for high temperature applications. These applications include but are not limited to semiconductor, smartcard, electronic, automotive and general manufacturing industries.
LINQTAPE PIT0.5S-DCD Series Film provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. It can be used in applications that may see temperatures up to 260°C (400°F).
LINQTAPE PIT0.5S-DCD polyimide tape can be delivered in a range of die cut disc sizes with diameters ranging from 1/8" to 12".