LAIRD LS-30

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

LAIRD LS-30

Main features

  • Compliant Polyurethane Foam Format
  • RF Isolation and Insertion Loss
  • Cavity Resonance Suppression

Product Description

Eccosorb LS-30 Polyurethane Foam Absorber is a lightweight dielectric foam stock material for managing RF and microwave energy in electronic assemblies. Its compliant polyurethane construction supports placement in cavities or between radiating structures where a non-rigid absorber format is preferred. The material is used to increase isolation, add insertion loss, and damp resonant energy within enclosed RF spaces. Applications include RF isolation, microwave attenuation, and cavity resonance suppression in communications equipment, test hardware, and other electronic structures.

Key features

  • Compliant Polyurethane Foam: A lightweight foam format supports placement in cavities and around irregular RF structures.
  • RF Isolation Support: The absorber is used to increase isolation and insertion loss between radiating elements.
  • Cavity Resonance Damping: Foam placement supports suppression of resonant energy in enclosed RF and microwave spaces.

Applications / Suitable for

  • RF isolation between electronic structures
  • Microwave insertion-loss applications
  • Cavity resonance suppression
Product Family

LAIRD LS-30

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Service temperatureService temperature
Max 90 °C

Additional Information

1910

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers