LAIRD ECCOSORB GDS

Harmonization Code : 3215907090 | Ink, whether or not concentrated or solid (excl. printing ink, printer/copier ink cartridges incorporating mechanical or electrical components, and solid ink in engineered shapes for printers/copiers)

LAIRD GDS

Main features

  • Thin Conformable Construction
  • High-Frequency RF Attenuation

Product Description

LAIRD Eccosorb GDS is a thin, flexible, magnetically loaded silicone rubber sheet for microwave absorption at frequencies of 18 GHz and above. The electrically non-conductive material is designed to function directly in front of metallic surfaces, where it can damp cavity resonances, reduce metal-surface reflectivity, and support isolation or attenuation within antenna and waveguide structures. Its silicone construction is impervious to moisture, withstands service temperatures up to 170 °C, and exhibits low outgassing for space-related applications. Standard material is supplied as a 305 × 305 × 0.76 mm sheet, with pressure-sensitive adhesive and custom configurations available.

Key features

  • High-frequency microwave absorption: Designed for operation at frequencies of 18 GHz and above.
  • Electrically non-conductive silicone: Volume resistivity greater than 1011 ohm-cm, combined with a flexible, moisture-impervious construction.
  • Low-outgassing, high-temperature performance: Reports 0.2% TML and 0.08% CVCM per ASTM E595-07, with a maximum service temperature of 170 °C.

Applications / Suitable for

  • Microwave cavity resonance damping
  • Antenna elements and microwave dishes
  • Waveguide isolation and attenuation
  • Metal-surface reflectivity reduction
  • Backscatter reduction from selected side or rear surfaces
Product Family

LAIRD ECCOSORB GDS

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers