Hysol GR180R | White Epoxy Mold Compound
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Main features
- Reflective compound
- High reliability
- Great workability
Product Description
Hysol GR180R is a white, reflective epoxy molding compound used for optical applications. This fused silica filled (76 - 86%) product has been specifically designed to improve light reflectance and workability for optocouplers also knows as photo-couplers, optical isolators, or opto-isolators.
Hysol GR180R cures with heat and has a filler cut size of 75um that is ideal for transfer processes. It has been formulated to provide the best possible moldability and for a wide range of molding process parameters.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Chemical Properties
Physical Properties
Curing Conditions
Additional Information
Storage
Store product in the unopened container in a dry location. Storage information may be indicated on the product container labeling.
Optimal Storage: 5°C or below, in closed containers. After removal from cold storage, the material MUST be allowed to come to room temperature, in the sealed container, to avoid moisture contamination. The suggested waiting time for a standard 15 kg carton box is 24 hours.