FREKOTE AC4368

Main features

  • Combined Mold Release and Conditioning
  • Multi-Resin Molding Compatibility
  • 5 to 10-Minute Solvent Evaporation

Product Description

LOCTITE® FREKOTE® AC4368 is a clear, one-part, silicone-based mold release agent containing a lubricant for release and mold-surface conditioning. The liquid can be brushed or sprayed onto clean metal or plastic mold surfaces, where the solvent evaporates to leave a thin release film. It is suitable for molding processes using epoxy, polyurethane, and polyester materials with room-temperature or elevated-temperature cure systems.

Key features

  • Multipurpose release: Supports release applications involving epoxy, polyurethane, and polyester molding materials.
  • Surface conditioning: Contains a lubricant that conditions the mold surface while forming the release film.
  • Flexible application: Can be applied by brushing or spraying and used with room-temperature or elevated-temperature cure systems.

Applications / Suitable for

  • Release and conditioning of metal and plastic molds
  • Epoxy, polyurethane, and polyester molding systems
  • Room-temperature and elevated-temperature cure processes
Product Family

FREKOTE AC4368

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied characteristics and storage information for LOCTITE® FREKOTE® AC4368.

Property Value Unit Method / condition
Physical form Liquid As supplied
Appearance Clear Visual
Odor Hydrocarbon As supplied
Solvent Hexane Solvent carrier
Specific gravity 0.72 Typical product value
Shelf life 18 months From date of manufacture

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers