EPOCAP 43645

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

EPOCAP 43645

Main features

  • Two-Component Room-Temperature Epoxy
  • 7,000 psi Tensile Strength
  • 90-Minute Gel Time

Product Description

EPOWELD® 43645/53655 is a two-component, room temperature curing epoxy compound designed for general-purpose adhesive and casting applications. Formerly known as EPOWELD® 3645A/3655B, this versatile system delivers high mechanical strength and is particularly recommended for bonding components in demanding impact environments.

Key features

  • High-strength bonding: Delivers a robust tensile strength of 7,000 psi and a lap shear strength of 4,000 psi on aluminum.
  • Convenient processing: Features a simple 1:1 mix ratio by weight and cures fully at room temperature.
  • Extended working time: Offers a 90-minute gel time for a 100-gram mass, easily accommodating complex assembly or casting processes.

Applications / Suitable for

  • Bonding striking tools such as hammers, axes, and sledge hammers.
  • General-purpose adhesive applications.
  • General-purpose casting applications.
Product Family

EPOCAP 43645

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Amber
Specific GravitySpecific Gravity
1.06 g/cm³
Physical Properties
ViscosityViscosity
6,000 (Mixed) mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Pre-cure processing characteristics of mixed EPOWELD® 43645/53655.

Property Value Unit Method / condition
Appearance / Color (Mixed) Amber - -
Mix Ratio (Weight) 1:1 (100:100) - Part 43645 to Part 53655
Mix Ratio (Volume) 100:116 - Part 43645 to Part 53655
Viscosity (Mixed) 6,000 cps at 25°C
Specific Gravity (Mixed) 1.06 - at 25°C
Gel Time (100 gm mass) 90 minutes -
Gel Time (1.5 gal mass) 60 minutes -
Technical properties

After-processing / final-state properties

Typical cured mechanical and thermal properties of EPOWELD® 43645/53655 when cured for 7 days at 25°C.

Property Value Unit Method / condition
Hardness 82 Shore K Tested at 25°C
Tensile Strength 7,000 psi Tested at 25°C
Lap Shear Strength 4,000 psi Al/Al, tested at 25°C
Heat Distortion Temperature 55 °C Tested at 25°C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers