ELANTAS CE-1170
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- One-Component Acrylic Conformal Coating
- 15-Minute Tack-Free Time
- 2 x 10^15 ohm-cm Volume Resistivity
Product Description
CONAP® CE-1170 Acrylic Conformal Coating is a one-component, solvent-based acrylic conformal coating for printed circuit boards, epoxy-glass laminates, phenolic laminates, components, and other thin-film electronic applications. The coating is room-temperature or heat curable, with a typical tack-free time of 15 minutes, full cure in 24 hours at 25°C, or accelerated cure in 45 minutes at 60°C. It is documented as flexible, quick drying, repairable, humidity resistant, and hydrolytically stable, with a typical volume resistivity of 2 × 10¹⁵ ohm·cm.
Key features
- One-component acrylic coating: The solvent-based material is used for thin-film protection of components and printed circuitry.
- Fast handling: Typical tack-free time is 15 minutes, with room-temperature or accelerated heat cure.
- Electrical insulation: Typical volume resistivity is 2 × 10¹⁵ ohm·cm.
Applications / Suitable for
- Printed circuit boards and printed circuitry
- Epoxy-glass and phenolic laminates
- Thin-film coating of electronic components
TDS, SDS & Technical Documents
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical base | Acrylic | N/A | One-component solvent-based coating |
| Color | Amber | N/A | One-gallon can configuration |
| Specific gravity | 0.93 | N/A | As supplied |
| Viscosity | 400 | cP | As supplied |
| Tack-free time | 15 | min | Typical |
| Cure options | 24 h at 25°C; 45 min at 60°C | N/A | Room-temperature or heat cure |
| Flash point | 7 | °C | One-gallon can configuration |