LOCTITE ECCOBOND UV9060F

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND UV9060F

Main features

  • UV & Moisture Cure
  • Cures in shadowed areas
  • Translucent light blue

Product Description

LOCTITE ECCOBOND UV 9060F no flow encapsulant is designed for local circuit board protection as a UV curing coating/encapsulant with secondary moisture cure in shadow areas. This product is fluorescent when viewed with ultraviolet (black) light.

LOCTITE ECCOBOND UV 9060F is a one component, fast curable translucent material that is easily dispensed without stringing. It is fluorescent under UV light and it typically used for assembly applications and the local protection of WLCSP and BGA on circuit boards.

Product Family

ECCOBOND UV9060F

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 54 days
CA Shipping in 12 weeks
EU Shipping in 40 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
75 °C
Physical Properties
ViscosityViscosity
11,000 mPa.s

Additional Information

UV Cure

Light Source and Condition:

Metal halide doped spectrum UV lamp

  • Lamp Power, W/in 300
  • Distance between lamp to substrate, inches 4
  • Irradiance UVA, EIT puck radiometer, mW/cmÇ 566
  • Recommended Dose, seconds 5 to 25

Moisture cure occurs at ambient temperature and humidity.

*Cures at least 0.25 inch under optimum conditions.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers