LOCTITE ECCOBOND FP4655
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Main features
- Low stress
- Fine particle filler
- Combine with FP4451
Product Description
LOCTITE ECCOBOND FP4655 is a high-performance fill encapsulant that can be used alone as a cavity fill material, or in combination with FP4451 material as part of a dam and fill system. This low stress, self levelling epoxy has been used for Medical applications.
LOCTITE ECCOBOND FP4655 is based on the same chemistry as the FP4451 and, therefore, is completely compatible with that product. Its low viscosity and fine particle filler size make it ideal for devices with fine-pitch wire spacing. Dam and fill materials should be co-cured to obtain the best results.
Recommended Cure Schedule
- 15 minutes @ 110°C plus 30 minutes @ 165°C
- 30 minutes @ 125°C plus 90 minutes @ 165°C