DUROPTIX OE-6370

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

DUROPTIX OE-6370

Main features

  • 1:1 Optical Encapsulant Mixing
  • 100% Transparent Optical Protection
  • 240-Minute 150 deg C Cure

Product Description

DuPont Duroptix™ OE-6370 HF Optical Encapsulant is a colorless, two-part 1:1 mix silicone elastomer designed for LED encapsulation and overmolding applications. Based on a polydimethylsiloxane chemistry, this optical encapsulant combines high transparency, thermal stability, moisture resistance, and adhesion to commonly used LED substrates. The material provides excellent optical clarity with 100% transparency at 450 nm through a 1 mm sample thickness and is formulated to withstand the thermal demands associated with modern LED manufacturing processes. Its fast-curing characteristics and compatibility with standard dispensing and molding equipment support efficient production workflows for LED packaging and protection.

Key features

  • High optical transparency: Delivers 100% transparency at 450 nm (1 mm thickness) for light-transmission-critical LED applications.
  • Fast heat cure: Achieves cure in approximately 240 minutes at 150°C, supporting efficient LED encapsulation processes.
  • Thermally stable silicone elastomer: Provides durability across demanding operating environments and LED package thermal cycles.

Applications / Suitable for

  • LED encapsulation
  • LED package protection
  • Optical encapsulant applications
  • Overmolding processes
Product Family

DUROPTIX OE-6370

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Clear
Component SystemComponent System
2
Mix RatioMix Ratio
1 : 1
Refractive indexRefractive index
1.41

Additional Information

Technical properties

As-supplied / before-processing properties

Representative as-supplied properties for the two-part optical encapsulant system.

Property Value Unit Method / condition
Mix Ratio 1:1 - Two-part system
Color Clear - As supplied
Viscosity (Part A) 6100 cP Part A
Viscosity (Part B) 5300 cP Part B
Mixed Viscosity 5600 cP Mixed material
Shelf Life 12 months Stored at 35°C
Technical properties

After-processing / final-state properties

Representative cured optical and physical properties.

Property Value Unit Method / condition
Heat Cure Time 240 minutes 150°C
Hardness 70 Shore A JIS
Transparency at 450 nm 100 % 1 mm thickness
Refractive Index 1.41 - Typical value
Operational Temperature Range -45 to 200 °C General silicone operating range

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers