DOWSIL SE 9188

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

DOWSIL SE9188

Main features

  • 10-Minute Tack-Free Time
  • 2.9 MPa Cured Tensile Strength
  • UL 94 V-0 Classification

Product Description

DOWSIL™ SE 9188 RTV Adhesive is a one-part, gray, non-flowing polydimethylsiloxane adhesive for room-temperature bonding, fixing, vibration dampening, and sealing in electronics assemblies. The material requires no mixing and has a typical tack-free time of 10 minutes at 25°C, with optional mild heat acceleration. It is documented with controlled silicone volatility and a UL 94 V-0 flammability classification. Typical cured properties include Shore A 34 hardness, 2.9 MPa tensile strength, 400% elongation, 30 kV/mm dielectric strength, and 1.0 × 10¹⁵ ohm·cm volume resistivity.

Key features

  • Non-flowing one-part RTV: The gray adhesive remains in place and requires no component mixing.
  • Fast tack-free cure: Typical tack-free time is 10 minutes at 25°C.
  • Documented flame classification: The product is listed with UL 94 V-0 flammability classification.

Applications / Suitable for

  • Part fixing on circuit boards
  • Vibration dampening
  • Electronic sealing applications
Product Family

DOWSIL SE 9188

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Product form One-part non-flowing RTV adhesive N/A As supplied
Color Gray N/A As supplied
Tack-free time 10 min At 25°C
Low-molecular siloxane content 30 ppm D4-D10
Low-molecular siloxane content 220 ppm D4-D20
Technical properties

After-processing / final-state properties

Typical cured, installed, or in-use values under the stated conditions. These values are not sales specifications.

Property Value Unit Method / condition
Cured specific gravity 1.29 N/A Typical cured value
Hardness 34 Shore A Typical cured value
Tensile strength 2.9 MPa Typical cured value
Elongation 400 % Typical cured value
Dielectric strength 30 kV/mm Typical cured value
Volume resistivity 1.0 × 10¹⁵ ohm·cm Typical cured value
Dielectric constant 3.4 N/A At 1 MHz
Flammability classification V-0 UL 94 Documented classification

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers