DOWSIL SE 9184
Harmonization Code : 3215907090 | Ink, whether or not concentrated or solid (excl. printing ink, printer/copier ink cartridges incorporating mechanical or electrical components, and solid ink in engineered shapes for printers/copiers)

Main features
- Fast Tack-Free Rt Cure
- Non-Sag Placement Control
- Thermally Conductive Thermal Bonding
Product Description
DOWSIL™ SE 9184 RTV Adhesive is a one-part, non-flowing, thermally conductive RTV silicone adhesive designed to provide both adhesion and heat transfer for cooling electrical and electronic components. The moisture-cure material offers fast tack-free performance at room temperature without requiring mixing or oven curing, helping support efficient assembly processes. Its thermally conductive formulation, controlled silicone volatility, and UL 94 V-0 flammability classification make it suitable for applications where thermal management and flame resistance are important considerations. The cured elastomer provides durable adhesion while maintaining electrical insulation properties.
Key features
- Fast room-temperature cure: Tack-free in approximately 3 minutes with no mixing or oven curing required.
- Thermal conductivity: Thermal conductivity of 0.84 W/m·K supports heat transfer from electronic components to thermal management systems.
- Flame-resistant formulation: UL 94 V-0 classification and controlled silicone volatility support demanding electronic assembly environments.
Applications / Suitable for
- Thermal management of electrical and electronic components
- Bonding applications requiring heat dissipation
- PCB system assemblies
- Consumer electronic devices with compact designs
- Applications requiring thermal transfer and added flame resistance
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Typical properties of the adhesive before cure and processing. Values are typical data and not intended as specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product type | One-part | - | As supplied |
| Color | White | - | As supplied |
| Non-volatile content | 98.9 | % | Typical value |
| Tack-free time | 3 | minutes | 25°C |
| Physical form | Paste | - | SDS appearance data |
After-processing / final-state properties
Typical cured properties. Values are typical data and not intended as specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Thermal conductivity | 0.84 | W/m·K | Typical cured property |
| Tensile strength | 3.2 | MPa | Typical cured property |
| Elongation | 60 | % | Typical cured property |
| Hardness | 74 | Shore A | JIS standard |
| Lap shear adhesion to aluminum | 1.7 | MPa | Unprimed adhesion |
| Dielectric strength | 20 | kV/mm | Typical cured property |
| UL flammability classification | 94 V-0 | - | UL classification |