Product Description

DOWSIL™ SE 1720 CV Adhesive Kit is a two-part, white, flowable silicone adhesive with a 1:1 mix ratio and controlled volatility for electronic assembly processes. The solvent-free material may be dispensed manually or automatically and has a typical mixed viscosity of 89,700 cP with a six-hour working time at 25°C. Documented cure schedules range from 50 minutes at 70°C to 10 minutes at 100°C. Applications include sealing ceramic condensers and printed circuit-board module components and bonding computer keypad assemblies. Typical cured properties include 3.3 MPa tensile strength, 375% elongation, and Shore A 33 hardness.

Key features

  • Flowable 1:1 system: The two-part adhesive supports manual or automated needle dispensing.
  • Moderate-temperature cure: Documented cure schedules range from 50 minutes at 70°C to 10 minutes at 100°C.
  • Controlled-volatility elastomer: Typical cured data include 3.3 MPa tensile strength and 375% elongation.

Applications / Suitable for

  • Sealing ceramic condensers
  • Sealing printed circuit-board module components
  • Bonding computer keypad assemblies
Product Family

DOWSIL SE 1720

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Color White N/A As supplied
Mix ratio 1:1 ratio Part A : Part B
Viscosity, Part A 37,700 cP Typical
Viscosity, Part B 41,900 cP Typical
Mixed viscosity 89,700 cP Typical
Working time 6 h At 25°C
Heat cure 50 min at 70°C; 30 min at 80°C; 10 min at 100°C N/A Documented schedules
Technical properties

After-processing / final-state properties

Typical cured, installed, or in-use values under the stated conditions. These values are not sales specifications.

Property Value Unit Method / condition
Cured specific gravity 1.06 N/A Typical cured value
Tensile strength 3.3 MPa Typical cured value
Elongation 375 % Typical cured value
Tensile modulus 0.9 MPa Typical cured value
Hardness 33 Shore A JIS
Lap shear adhesion 1.6 MPa Unprimed aluminum

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers