DOWSIL 3-6060

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

DOWSIL 3-6060

Main features

  • Improved Inhibition Resistance
  • Promotes Bonding to Most Plastics
  • Wipe, Dip, or Spray Application

Product Description

DOWSIL™ 3-6060 Prime Coat is a one-part, solvent-based silicone surface treatment formulated to improve inhibition resistance and promote bonding for selected addition-cure and peroxide-cure silicone materials. The clear-to-yellow liquid is suitable for most plastics, ceramics, composites, and metals. It is applied as a very light, even coating by wiping, dipping, or spraying, then allowed to react with atmospheric moisture before the silicone material is applied.

Key features

  • Improved inhibition resistance: Formulated to improve inhibition resistance when processing compatible addition-cure silicone products.
  • Broad substrate suitability: Supports bonding to most plastics, ceramics, composites, and metals.
  • Compatible silicone systems: Intended for use with selected two-part addition-cure and peroxide-cure silicone materials.
  • Multiple application methods: May be applied in a very light, even coat by wiping, dipping, or spraying.

Applications / Suitable for

  • Priming most plastics, ceramics, composites, and metals
  • Improving inhibition resistance for compatible addition-cure silicone products
  • Promoting adhesion of selected two-part addition-cure and peroxide-cure silicones
Product Family

DOWSIL 3-6060

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
liquid

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied and processing properties. Values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Product form One-part liquid prime coat Dilute solution of silane coupling agents and other active ingredients
Color Clear to yellow As supplied
Solvent MIBK Methyl isobutyl ketone carrier solvent
Flash point, closed cup 15 (59) °C (°F) Dow Corning Corporate Test Method 0917, based on ASTM D 3278
Volatile organic content 780 g/L Typical value
Typical cure time 1–2 hours Room temperature and 20–90% relative humidity; lower temperature or humidity requires longer cure
Shelf life 12 months From date of manufacture; store below 32°C (90°F) and protect from moisture

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers