CONAP AD-1146-C

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

CONAP AD-1146-C

Main features

  • Lower-Viscosity Amber Adhesive-Primer Variant
  • Liquid-Polyurethane Bonding on Supported Substrates
  • Two-Coat Drying and Activation Process

Product Description

CONAP AD-1146-C Adhesive Primer is a distinct amber, lower-viscosity variant in the AD-1146 primer series for priming supported substrates before liquid-polyurethane bonding. The documented process uses two primer coats with controlled surface preparation, drying, and heat activation before the polyurethane is applied. The lower-viscosity AD-1146-C grade should remain distinct from AD-1146 during selection and processing. Applications are limited to the supported substrate and liquid-polyurethane bonding combinations documented for this exact variant.

Key features

  • Flow and dispensing: Distinct lower-viscosity amber AD-1146-series primer variant.
  • Application fit: Designed for priming supported substrates before liquid-polyurethane bonding.
  • Processing sequence: Two-coat application with controlled drying and heat activation.

Applications

  • Liquid-polyurethane bonding
  • Supported substrates
  • Variant-specific processes
Product Family

CONAP AD-1146-C

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Amber
SolidsSolids
13-15 %
Physical Properties
ViscosityViscosity
125-225 mPa.s
Thermal Properties
Flash PointFlash Point
10 °C

Additional Information

SURFACE TREATMENT

CONAP AD-1146-C lower-viscosity adhesive primer

A distinct amber, lower-viscosity variant in the AD-1146 primer series. documented product information position AD-1146-C for priming supported substrates before liquid-polyurethane bonding and specify a two-coat application with controlled drying and activation before the polyurethane is applied. The variant is intended to keep the primer process distinct from the higher-viscosity AD-1146 grade.

Adhesive primerAmberLower viscosityTwo-coat process

AS-SUPPLIED PROPERTIES

Variant-specific product characteristics

Keep AD-1146-C properties and process controls separate from the related AD-1146 grades.

Property Value Condition
Product type Adhesive primer As supplied
Appearance Amber As supplied
Variant characteristic Lower viscosity than AD-1146 Series comparison
Bonding role Primer before liquid-polyurethane bonding Supported substrate systems

PROCESSING

Two-coat primer process

The two-coat AD-1146-C process uses controlled surface preparation, drying, activation, and polyurethane application.

  1. Prepare the supported substrate surface.
  2. Apply the first AD-1146-C primer coat.
  3. Dry or activate according to the controlled technical process.
  4. Apply the second primer coat and complete the documented drying / activation sequence before polyurethane application.

Process boundary

Do not substitute AD-1146 single-grade values or application instructions without confirming that they are explicitly stated for AD-1146-C.

TECHNICAL GUIDANCE

Maintain variant-specific process control

The lower-viscosity AD-1146-C grade should be evaluated on its own process record rather than treated as interchangeable with AD-1146.

Variant identity

Use the exact AD-1146-C designation in material, work-instruction and traceability records.

Coat sequence

Maintain the documented two-coat process and controlled drying / activation sequence.

System validation

Confirm the complete substrate, primer and liquid-polyurethane combination under the intended production conditions.

APPLICATIONS

Documented application context

AD-1146-C is documented for priming supported substrates before bonding with liquid polyurethane systems.

Liquid-polyurethane bonding

Use as a surface primer in documented liquid-polyurethane bonding systems.

Supported substrates

Apply only to substrate classes covered by the exact AD-1146-C technical record.

Variant-specific processes

Use where the lower-viscosity AD-1146-C variant and its two-coat process are appropriate to the controlled assembly.

Discuss your application with Krayden

For AD-1146-C evaluation, provide the substrate, surface preparation, polyurethane system and required application method so Krayden can help review the variant-specific two-coat primer process for your assembly. Krayden can also help review the documented processing conditions and evaluation criteria before testing.

Contact Us

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers