BOSTIK LADH1531AC

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

BOSTIK LADH1531AC

Main features

    Product Description

    Bostik LADH1531AC is a solvent-based neoprene contact adhesive designed for high-speed spray application in veneer bonding and other industrial laminating processes. The sprayable formulation delivers excellent green strength for immediate handling while providing high water, oil, and heat resistance after bonding. It is formulated for large-area, uniform adhesive coverage, enabling rapid processing and reduced production time in industrial manufacturing environments. :contentReference[oaicite:0]{index=0}

    Key Features

    • Sprayable neoprene contact adhesive for rapid, uniform adhesive application.
    • Excellent green strength allows immediate handling after bonding.
    • High water, oil, and heat resistance for demanding industrial applications.
    • Designed for fast production with quick bond development for high-speed manufacturing.

    Applications / Suitable For

    • Veneer bonding
    • Industrial laminating
    • High-speed spray bonding
    • Large-area contact bonding
    • General industrial assembly
    Product Family

    BOSTIK LADH1531AC

    Catalog Product

    Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

    TDS, SDS & Technical Documents

    Technical Specifications

    General Properties
    Process MethodProcess Method
    Solvent evaporation
    Product TypeProduct Type
    Solvent-based neoprene contact adhesive
    Thermal Properties
    Operating TemperatureOperating Temperature
    Drying at 80°C °C

    Additional Information

    Technical Properties

    As-Supplied / Before-Processing Properties

    Property Value Unit Method / Condition
    Product type Neoprene solution contact adhesive Sprayable solvent-based adhesive
    Appearance Tan liquid Typical physical property
    Total solids 16 % Typical value
    Viscosity 185 cP LVF #2 @ 60 rpm, 25°C
    Density 6.7 lb/gal Typical value
    Flash point (SCC) -22 (-30) °F (°C) Typical value
    Shelf life 270 days (9 months) Stored between 55–100°F (13–38°C)
    Technical Properties

    After-Processing / Final-State Properties

    Property Value Unit Method / Condition
    Dry adhesive coat weight 2–5 g/ft² Applied to both substrates
    Recommended drying condition 80 °C 1–3 minutes in circulating air oven
    Press pressure 7 (0.5) psi (kg/cm²) 10–15 seconds for contact bonds
    Green strength Adequate for immediate handling After recommended bonding process
    Performance High water, oil and heat resistance Supplier description

    Leading Brands Trust in Our Products and Services

    • Jabil
    • Linxens
    • Magna
    • Medtronic
    • NXP
    • Philips
    • Semikron
    • Teledyne
    • Thales
    • Vishay
    • ZF
    • AMS
    • Apple
    • Audi
    • Broadcom
    • Borgwarner
    • Bosch
    • Eaton
    • Henkel
    • Honeywell
    • Hysol
    • Intel
    Products that Perform|Knowledge that Serves|Service that Delivers