BOSTIK L1007M
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

Main features
- Broad-Substrate Adhesion Primer
- Fast-Drying Heat-Resistant Base Coat
- Metal/Plastic/Glass/Wood Surface Priming
Product Description
Bostik 1007M Primer is a general-purpose, solvent-based synthetic resin primer designed to improve the adhesion of subsequently applied adhesives and coatings. It forms a firm base coat that enhances bonding efficiency while providing good heat resistance and bond flexibility. Developed as a replacement for Bostik 1007P Primer with improved container stability, it is suitable for preparing metals, plastics, glass, wood, concrete, and other rigid or semi-rigid substrates used across the aerospace, automotive, construction, electronics, plastics, rubber, and textile industries. :contentReference[oaicite:0]{index=0}
Key Features
- General-purpose adhesion primer improves the anchorage of adhesives and coatings on a wide variety of substrates.
- Fast drying to the touch in approximately one hour at room temperature.
- Good heat resistance and bond flexibility for demanding industrial applications.
- Improved storage stability developed as a replacement for Bostik 1007P Primer.
Applications / Suitable For
- Priming metal or concrete tanks, vats and ducts before installation of semi-rigid PVC liners
- Primer for bonding synthetic rubber de-icing equipment to aircraft wings and propellers
- Priming fiberglass reinforced plastics and metals before applying neoprene coatings
- Surface preparation for metals, plastics, glass, wood and concrete prior to adhesive bonding
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-Supplied / Before-Processing Properties
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Product type | Solvent-based synthetic resin primer | — | General-purpose primer |
| Appearance | Yellow/brown thin syrup | — | Typical physical property |
| Base | Neoprene | — | Typical composition |
| Solvent | Bostik 3302 Solvent, toluene | — | Typical composition |
| Viscosity | 75–400 | cP | Typical physical property |
| Density | 7.9 lb/gal (1.0 kg/L) | — | Typical physical property |
| Solids content | Approximately 27 | % | Typical physical property |
| Flash point (SCC) | 20 (-7) | °F (°C) | Typical physical property |
| Shelf life | 9 months | — | Stored at 22 ± 5°C (70 ± 10°F) |
After-Processing / Final-State Properties
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Drying time | Approximately 1 | hour | Room temperature |
| Primary function | Provides a firm base coat to maximize adhesive and coating bond efficiency | — | Supplier description |
| Heat resistance | Good | — | Supplier description |
| Bond flexibility | Good | — | Supplier description |
| Typical substrates | Metal, plastic, glass, wood, concrete, fiberglass reinforced plastic | — | Supplier description |