BOSTIK 6363
Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

Main features
- Wide-Range Hot-Melt Viscosity Control
- High-Temperature Service Range to 204 deg C
- Standard 0.5 in Glue-Gun Stick Format
Product Description
Bostik Thermogrip 6363 Hot Melt Adhesive is a one-part, medium-setting, general-purpose ethylene vinyl acetate (EVA) hot-melt adhesive supplied in off-white 0.5 in x 15 in sticks. It cures by cooling at room temperature after application and is typically used for furniture repair and assembly, leather products, component staking on PC boards, and automotive assembly or repair. The adhesive has a service temperature of 176.7 to 204.4 deg C and a flash point above 204.4 deg C, with Brookfield viscosity decreasing from about 33,500 cP at 162.8 deg C to about 8,875 cP at 204.4 deg C as application temperature increases. It is supplied in 25 lb cases of sticks for use with compatible hot-melt glue guns or applicators.
Key features
- EVA Hot-Melt Chemistry: one-part ethylene vinyl acetate hot-melt adhesive that cures by cooling at room temperature
- Application Viscosity Range: viscosity decreases from about 33,500 cP at 162.8 deg C to about 8,875 cP at 204.4 deg C
- 0.5 in x 15 in Glue-Gun Sticks: supplied in off-white sticks sized for standard hot-melt glue guns and applicators
Applications
Furniture repair and assembly, leather products, component staking on PC boards, and automotive assembly or repair.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Off-white | - | As supplied |
| Chemical composition | EVA (ethylene vinyl acetate) | - | As supplied |
| Cure system | Room temperature | - | Cooling after application |
| Flash point | greater than 204.4 | deg C | As reported |
| Service temperature | 176.7 to 204.4 | deg C | Application / service range |
| Viscosity | 33,500 to 8,875 | cP | Brookfield, 162.8 to 204.4 deg C, decreasing with temperature |