BIOACT EC-78
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

Main features
- RMA/No-Clean/Lead-Free Flux Removal
- Low-Foaming Electronics Cleaning
- Saponifier and Corrosion-Inhibitor Formulation
Product Description
BIOACT™ EC-78 Aqueous Batch Defluxer is a concentrated, inherently low-foaming aqueous cleaner formulated with water-dilutable solvents, specialty saponifiers, and corrosion inhibitors. Designed for extended cleaning cycles in batch spray-in-air equipment, it removes a broad range of solder-flux residues while helping protect electronic assembly surfaces. The formulation operates without added defoamers or anti-tarnishing agents and is typically used at concentrations of 5% to 25%.
Key features
- Broad flux-residue removal: Formulated to remove RMA, no-clean, lead-free, and water-soluble solder-flux residues.
- Inherently low foaming: Supports the high temperatures and extended spray cycles commonly used in batch washers.
- Integrated corrosion protection: Contains corrosion inhibitors to help protect electronic assembly surfaces during cleaning.
- No supplemental additives required: Does not require added defoamers or anti-tarnishing agents to maintain cleaning performance.
Applications / Suitable for
- Aqueous batch spray-in-air cleaning equipment
- Defluxing printed circuit board assemblies
- Removal of RMA, no-clean, lead-free, and water-soluble flux residues
- Extended-cycle batch washing processes
TDS, SDS & Technical Documents
Technical Specifications
Thermal Properties
General Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Typical as-supplied and recommended process properties. Values are not intended for use as specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product type | Concentrated aqueous batch defluxer | — | Water-dilutable formulation |
| Formulation | Water-dilutable solvents, specialty saponifiers, and corrosion inhibitors | — | As supplied |
| Odor | Mild | — | As supplied |
| Flash point | None to boiling | — | Reported in the supplied TDS |
| Specific gravity | 0.944 | — | At 25°C |
| Viscosity | 16 | cps | At 25°C |
| pH | 10.1 | — | 15% concentration |
| Recommended use concentration | 5–25 | % | Batch spray-in-air cleaning |
| Recommended operating temperature | 120–160 (50–70) | °F (°C) | Batch spray-in-air cleaning |