AXAREL 32
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

Main features
- Water-Rinsable pH-Neutral Electronics Cleaning
- Ionic/Flux/Oil Contamination Removal
- Ambient to 71 deg C Defluxing
Product Description
AXAREL™ 32 Water Rinsable Immersion Cleaner & Defluxer is a pH-neutral cleaning mixture formulated with highly refined solvents and surfactants for immersion cleaning of electronic components and assemblies. Designed for temperature-flexible defluxing, it removes ionic contamination, high-temperature flux residues, oils, and other manufacturing contaminants. The water-rinsable formulation is supplied ready to use and can be applied at full concentration in immersion cleaning processes from ambient temperature up to 71°C (160°F).
Key features
- Water-rinsable formulation: Supports removal of the cleaning solution and dissolved contaminants through a subsequent water-rinse process.
- pH-neutral cleaner: Provides a neutral cleaning formulation for electronic component and assembly cleaning.
- Temperature-flexible defluxing: Suitable for immersion cleaning from ambient temperature up to 71°C (160°F).
Applications / Suitable for
- Immersion cleaning of electronic components and assemblies
- Removal of ionic contamination
- Removal of high-temperature flux residues
- Removal of oils and other manufacturing contaminants
TDS, SDS & Technical Documents
Technical Specifications
Thermal Properties
General Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Typical properties of AXAREL™ 32 before use.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Formulation | Highly refined solvents and surfactants | — | As supplied |
| pH classification | Neutral | — | Typical |
| Flash point | 96 (205) | °C (°F) | Typical |
| Specific gravity | 0.85 | — | 25°C |
| Viscosity | 2.8 | cP | 25°C |