ARALDITE LY5052

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ARALDITE LY5052

Main features

  • Low-Viscosity Composite Processing
  • Multiple Composite Process Routes
  • Tooling and Repair System Fit

Product Description

ARALDITE LY 5052 Epoxy Resin is a low-viscosity epoxy resin component for composite laminating and infusion systems used with ARADUR 5052 hardener. The resin supports wet lay-up, resin-transfer molding, pressure molding, filament winding, tooling, and composite repair within the specified two-part system. Its component role provides the resin base for controlled mix ratios and processing windows defined for the complete formulation. LY 5052 is sold separately, so cure behavior and final composite properties remain tied to ARADUR 5052, the selected ratio, the manufacturing process, and the stated cure schedule. This distinction keeps component handling separate from cured-system performance.

Key features

  • Low-viscosity resin processing: The LY 5052 component is specified for laminating and infusion workflows.
  • Multiple composite process routes: The complete system supports wet lay-up, RTM, pressure molding, and filament winding.
  • Tooling and repair system: LY 5052 with ARADUR 5052 is used for composite tooling and repair.

Applications

Wet lay-up, resin-transfer molding, pressure molding, filament winding, tooling, and composite repair within the LY 5052/ARADUR 5052 system.

Product Family

ARALDITE LY5052

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
clear liquid
Density (g)Density (g)
1.17 g/cm3
Physical Properties
ViscosityViscosity
1000-1500 mPa.s
Thermal Properties
Flash PointFlash Point
140 °C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers