LOCTITE ABLESTIK ICP 8282
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- Snap cure
- High flexibility
- High speed print
Product Description
LOCTITE ABLESTIK ICP 8282 is an electrically conductive acrylate adhesive designed for applications where fast cure is required. This single component, snap cure material is ideally suited for high throughput photovoltaic print processes and applications where high adhesion strength is required.
LOCTITE ABLESTIK ICP 8282 achieves low and stable contact resistance on noble metallisation during reliability testing. It has low silver content that reduces its density making it a very cost effective conductive material compared to similar fast cure products such as CA 3556HF. It is typically used for flexible interconnects in photovoltaic and solar panel shingle applications and also on stencil printing processes that need to print at high speeds and high volumes.
Snap Cure
- 10 to 15 seconds @ 150°C
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Electrical Properties
Physical Properties
Additional Information
Protip
By applying a flat and thin 100-200um layer using JET dispensing or STENCIL printing (instead of one domed dot), we believe that the flow out and bleeding can be reduced by lower gravity forces.