LOCTITE ABLESTIK CDF 530P

Harmonization Code : 7115.90.00.00 | Other articles of precious metal or of metal clad with precious metal : Other

LOCTITE ABLESTIK CDF 530P

Main features

  • Electrically conductive
  • Thermally conductive
  • QFN, TQFP, eTQFP

Product Description

LOCTITE ABLESTIK CDF 530P,  highly filled, conductive die attach adhesive is designed to provide high thermal and electrical conductivity in the attachment of integrated circuits and components onto metal leadframes. This adhesive exhibits strong adhesion to various wafer metallizations and leadframe finishes. It can be used in a variety of die sizes ranging from 3mm x 3mm to 8mm x 8mm .

LOCTITE ABLESTIK CDF 530P offers high MSL reliability, controlled fillet size and does not exhibit resin bleed out. It has good wetting and low warpage on large dies and is recommended for thin wafer handling applications. It comes in 15 (CDF 515P) and 30um and is typically used for QFN, TQFP and eTQFP package applications.

Cure Schedule

  • 30 minute ramp from 25°C to 200°C, hold 60 minutes @ 200°C
  • 30 minute ramp from 25°C to 175°C, hold 60 minutes @ 175°C
Product Family

ABLESTIK CDF530P

1. Select Package Type
2. Select Pieces per roll
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 20 days
CA Shipping in 12 weeks
EU Shipping in 35 days
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
5 °C
Thermal ConductivityThermal Conductivity
1.8 W/m.K
Electrical Properties
Volume ResistivityVolume Resistivity
0.0004 Ohms⋅cm
General Properties
Film ThicknessFilm Thickness
30 µm
Work life @25°CWork life @25°C
2160 hours

Additional Information



 
 

CDF 500P - Die attach film property comparison

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers