LOCTITE ABLESTIK ABP 2030SCR

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite ABP 2030SCR

Main features

  • Low moisture uptake
  • Low stress
  • Solvent free

Product Description

LOCTITE® ABLESTIK ABP 2030SCR silver filled conductive die attach adhesive has been formulated for use in high throughput die attach applications. This material is designed to minimize stress and resulting warpage between dissimilar surfaces. It can be used in a variety of package sizes. Another interesting property is that it exhibits lower strength at higher temperatures for easier chip removal.

LOCTITE® ABLESTIK ABP 2030SCR is a hybrid, snap cure, low stress product that is typically used for smart cart applications. It is the improved and latest version that supersedes 2030SC and 2030SCM.

Cure Schedule

  • 120 seconds @ 120°C 
  • 10 seconds @ 150°C
Product Family

ABLESTIK ABP2030SCR

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 35 days
CA Shipping in 12 weeks
EU Shipping in 35 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°CWork life @25°C
24 hours
Thermal Properties
Thermal ConductivityThermal Conductivity
2 W/m.K
Electrical Properties
Volume ResistivityVolume Resistivity
0.0002 Ohms⋅cm
Physical Properties
Thixotropic indexThixotropic index
5.0
ViscosityViscosity
15,000 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers